SOLSTICE PTM6000HV

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

PTM6000HV-SP | Phase Change Paste

Main features

  • 0.14 Thermal Impedance
  • 5.2 Thermal Conductivity
  • Optimized for IGBT

Product Description

PTM6000HV, commonly known as PTM6000HV, is a highly thermally conductive Phase Change Material (PCM) in paste format. This High viscosity(HV) version of PTM6000-SP is designed to minimize thermal resistance at interfaces and maintain extremely stable performance through reliability testing required for long product life applications. It has a very wide process window that makes it an optimal, tailor made option for IGBT printing and honeycomb structures.

PTM6000HV is based on a robust polymer PCM structure and exhibits excellent wetting properties during typical operating temperature ranges, resulting in very low surface contact resistance. This material exhibits excellent wetting at interfaces during typical operating temperature range, resulting in very low surface contact resistance.

PTM6000HV is a proprietary material that uses a proprietary filler to provide superior reliability (pass 150˚C baking 2000 hours, temperature cycling 2000 cycles, and HAST 288 hours) and maintains low thermal impedance (<0.12˚Ccm2/W no shim), making PTM6000HV desirable for high-performance integrated circuit devices. PTM6000HV has been renamed from PTM6000HV-SP for the sake of simplicity. It is the exact same product.

Reference the PTM6000 Automotive Reliability Report which demonstrates its performance and thermal stability after various long-term reliability tests including HAST 192hrs, T/C-B 4000x and High Temperature Baking of 3000hrs.

Product Family

231577

1 kg - Jar | Phase Change Paste
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 10 x 8 x 8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.6
Thermal Properties
Specific Heat Capacity
Specific heat capacity is the amount of heat energy required to raise the temperature of a substance per unit of mass. The specific heat capacity of a material is a physical property. It is also an example of an extensive property since its value is proportional to the size of the system being examined.
0.97 J/g.K J/(g⋅°C)
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
5.2 W/m.K
Thermal Impedance
0.09 °C·cm²/W
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
210000000000000 Ohms⋅cm

Additional Information

When choosing a printable paste it is important to understand the process parameters and limitations.

That's why we ask, when you contact us, to include  the following information:

  1. What is your print thickness?
  2. How long is your printing time and working window?
  3. What is your drying step after printing?
    • Temperature (Room temperature or something else?)
    • Time 
  4. Do you have any viscosity limitations in the printing process?
 
Product Use
Clamping pressure and temperature are suggested to achieve a minimum bond line thickness of the thermal interface material, typically less than 1.5 mil (0.038mm) for best performance.
The material must go through the phase change temperature to exhibit entitlement performance.
 
 
THERMAL IMPEDANCE POST RELIABILITY
(ASTM E1461)
 
End of Line
0.10 °C-cm²/W
 
Bake 125˚C, 2000 h 0.09 °C-cm²/W
Bake 150˚C, 2000 h 0.09 °C-cm²/W
HAST, 288h 0.09 °C-cm²/W
Temperature Cycling “B” 
(-55˚C to +125˚C, 2000 cycles)
0.07˚ °C-cm²/W
 
 
alt
Formulated specifically for IGBT modules assembly
 
The material is Optimized for IGBT printing and honeycomb structures with wider process time of >30 minutes. This material's high viscosity helps with printing and application in honeycomb structures, while its wide process window allows for easier and more reliable assembly of power modules in applications like inverters.
 

 
 
PTM6000HV is available as 650g (280cc Al cartridge) or 1000g (1 kg can). We also have 2 kg cans and 5 gallon pails if larger configurations are desired. All other printable pastes are available in these two same configurations since the densities of printable PCM paste fall in the range of 2.0 – 2.7 g/cc.



280cc cartridges are intentionally about 90% filled (650g) to allow for room at the top to fit the adaptor/plunger for dispensing.

Other lower filled configurations in 280cc cartridges are possible, if there is sufficient volume or justified with manufacturability concerns.
  

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers