LOCTITE DSP190024

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE DSP 190024

Main features

  • UV Cure
  • Bone white translucent
  • Sealant for displays

Product Description

LOCTITE® DSP 190024 is an acrylated urethane, primarily designed for bonding rigid and flexible PVC to polycarbonate where large gap filling capabilities (0.25mm) and a flexible joint are desired. Its flexibility enhances the load bearing and shock absorbing characteristics of the bond area. The product has shown excellent adhesion to a wide variety of substrates including glass, many plastics and most metals and is used as a UV curable sealant for displays. In that sense it is quite similar to LOCTITE 3703. The thixotropic nature of LOCTITE® DSP 190024™ reduces the migration of liquid product after application to the substrate.

LOCTITE® DSP 190024 can be cured by exposure to UV and/or visible light of sufficient intensity. Surface cure is enhanced by exposure to UV light in the 220 to 260 nm range. Cure rate and ultimate depth of cure depend on light intensity, spectral distribution of the light source, exposure time and light transmittance of the substrate through which the light must pass.

Product Family

214267

1 L - Bottle | White
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 25 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Unit of measure Bottle
Net weight 1.08 kg
Gross weight 1.17 kg
Dimensions 12.4 x 12.4 x 17.8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.12
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
85 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
20,000 mPa.s

Additional Information

Fixture Time

UV fixture time is defined as the light exposure time required to develop a shear strength of 0.1 N/mm2.

UV Fixture Time, Glass microscope slides, seconds:

  • 6 mW/cmÇ, measured @ 365 nm ≤10LMS

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers