LINQCELL GDP340 | 340um Non woven Carbon Paper

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

GDP340 | 340um Carbon Paper

Main features

  • 0.34mm - 340um - 13.4mil
  • Non woven
  • Highly flexible - Roll form

Product Description

LINQCELL GDP340 is a non woven carbon paper with a Microporous layer and PTFE. It is commonly used as a gas diffusion layer and electrode for fuel cells. Its through-plane resistivity is less than 10 mΩcm2. The thickness can reach 0.18mm at 1mPa. This carbon paper is highly flexible and has excellent air permability.

LINQCELL GDP340 is a close alternative to the discontinued Spectracarb 1550. This gas diffusion layer can be compressed ~50% at 100kPa. It is the only product that comes in long roll form.

Product Family

233738

400 x 400mm Sheet
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Sheet
Net weight 0.0979 kg
Gross weight 0.1077 kg
Dimensions 40 x 40 x 0.034 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
90 g/m2
Mechanical Properties
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
3 N/cm
Chemical Properties
Air Permeability
The air permeability of a fabric is a measure of how well it allows the passage of air through it.
40 cm3/s/cm2